Jul 21, 2025 Leave a message

What Is P235GH Pipe Material? EN 10216-2 Boiler Tube Grade Explained

What P235GH Pipe Material Is

P235GH is a non-alloy steel grade intended for elevated temperature service, specified for seamless tubes in EN 10216-2, the part of the European tube standard that covers non-alloy and alloy steel tubes with specified elevated temperature properties. It is also standardised under material number 1.0345. The designation records the specified minimum yield strength of 235 MPa, and the letters GH mark it as a grade intended for heat and pressure duty.

In practice P235GH is bought as seamless tube for boiler walls, superheater support tubes, heat exchanger bundles, feedwater heaters and general pressure piping where the design temperature is well above the limit normally accepted for ordinary carbon steel. Its attraction is a combination of adequate strength, good weldability, stable properties at temperature and a well understood specification for pressure equipment design.

Chemical and Mechanical Requirements

Element EN 10216-2 requirement for P235GH
Carbon (C) 0.16% max
Silicon (Si) 0.35% max
Manganese (Mn) 0.60 to 1.20%
Phosphorus (P) 0.025% max
Sulfur (S) 0.015% max
Aluminium (Al) 0.020% minimum for a fully killed, fine grain steel
Nitrogen (N) 0.012% max
Chromium, copper, nickel, molybdenum Residual limits individually specified in the standard
Property Requirement
Minimum yield strength at room temperature 235 MPa
Tensile strength 360 to 500 MPa
Elongation About 25% minimum longitudinal
Delivery condition Normalised or as specified in the standard
Elevated temperature data Proof strength values tabulated from 100 °C upwards

Behaviour at Elevated Temperature

What separates P235GH from a plain carbon steel tube is not room temperature strength but the data and the quality controls attached to it. EN 10216-2 tabulates the proof strength of the grade across the elevated temperature range, which allows a designer to carry out a proper pressure calculation rather than applying a blanket derating. The specification also fixes the deoxidation practice and the fine grain requirement, because a fine grained, fully killed steel keeps its toughness and its creep behaviour far better than a coarse grained one.

In boiler and heat exchanger service the practical upper temperature for P235GH is around 450 °C. Above that level the long term creep strength of a non-alloy steel becomes the limiting factor and a chromium bearing low alloy grade such as 13CrMo4-5 or 10CrMo9-10 is normally specified instead. Wall thickness range for the grade is wide, from thin heat exchanger tube up to heavy wall header tube, and the required wall is driven by the pressure calculation rather than by the grade alone.

Equivalent and Comparable Grades

P235GH is often compared with ASTM A106 Grade B for seamless pipe service and with ASTM A516 Grade 55 or 60 for plate applications, and with the Chinese boiler tube grades such as 20G under GB/T 3087. These comparisons are approximate: the phosphorus, sulfur and aluminium requirements differ between standards, and the elevated temperature data is tabulated differently in each system. For code governed work the grade called for by the design specification should be ordered and any substitution formally approved.

Fabrication, Testing and Common Pitfalls

P235GH welds readily by gas tungsten arc for the root and shielded metal arc, gas metal arc or submerged arc for fill and cap. Consumables should match the base metal strength and the design temperature, and heat input should be controlled to keep the heat affected zone tough. After forming, tube is normally supplied in the normalised condition so that a uniform, fine grained structure is present before the component is placed in service.

Ordering ordinary carbon steel tube where elevated temperature data is required by the design code.

Confusing P235GH with P265GH; the grades differ in carbon, manganese and strength level.

Overlooking the aluminium and nitrogen requirements that make the steel killed and fine grained.

Heat treating or welding in a way that coarsens the grain structure and destroys the elevated temperature advantage.

Applying P235GH above about 450 °C where creep strength rather than tensile strength governs.

FAQ

Q: What is P235GH pipe material?
P235GH is a non-alloy, fully killed steel grade for seamless tubes with specified elevated temperature properties, standardised in EN 10216-2 and known as material number 1.0345. It is used for boilers, heat exchangers and pressure piping.

Q: What is P235GH equivalent to in ASTM standards?
It is commonly compared with ASTM A106 Grade B for seamless pipe and with ASTM A516 Grade 55 or 60 for plate. The comparison is approximate because chemical limits and elevated temperature data differ between the two standards.

Q: What is the maximum service temperature of P235GH?
Around 450 °C in boiler and pressure equipment practice. Above that temperature creep strength governs and a chromium bearing low alloy grade is normally selected.

Q: What wall thickness is available in P235GH tube?
Production covers thin wall heat exchanger tubing through to heavy wall header tube. The required thickness is determined by the pressure design calculation, and dimensional limits follow EN 10216-2 for the ordered size.

Q: Is P235GH weldable?
Yes. It has low carbon and controlled impurities, so it welds with all common arc processes. Matching consumables and controlled heat input give a tough heat affected zone.

Q: What is the difference between P235GH and P265GH?
Both are EN 10216-2 non-alloy grades for elevated temperature service, but P265GH has a higher carbon and manganese content and a higher specified yield strength, so it suits slightly more highly stressed components.

Send Inquiry