Q235 and Q275 are two carbon structural steel grades from GB/T 700, the Chinese standard for hot-rolled carbon structural steels, and both are supplied as welded or seamless pipe for buildings, water transmission and general engineering. The letter Q stands for the Chinese word for yield, and the number that follows is the minimum yield strength in MPa, so Q235 guarantees at least 235 MPa and Q275 at least 275 MPa. Choosing between them, and between the quality grades that follow the number, decides strength, weldability and impact toughness.
How the GB/T 700 Designation Works
The designation is read from left to right and each part carries a fixed meaning:
Q – yield strength grade, from the Chinese term for yield point.
235 or 275 – minimum yield strength in MPa for the thinner thickness ranges.
A, B, C or D – quality grade, which sets the permitted phosphorus and sulfur content and the impact test requirement.
Optional suffix – a letter added by the mill or the purchaser to mark a deoxidation practice or a special requirement.
Q235 versus Q275
Both grades are non-alloy carbon steels; the difference is the strength level that the chemistry and the rolling practice deliver. Typical values for the thinner thickness range are shown below.
| Property | Q235 | Q275 |
|---|---|---|
| Minimum yield strength ReH | 235 MPa | 275 MPa |
| Tensile strength Rm | 370 to 500 MPa | 410 to 540 MPa |
| Minimum elongation | 26 % | 22 % |
| Carbon content | Lower | Higher, to reach the higher strength |
| Weldability | Excellent, the most forgiving of the two | Good, but thicker sections benefit from controlled welding procedure |
| Typical use | General structures, water pipe, scaffolding | Loaded members, vehicles, machinery frames, heavier pipe duties |
The practical trade-off is straightforward. Q275 carries more load per unit of section, which can save weight, but the higher carbon content reduces ductility and makes welding slightly less forgiving. Where a structure is welded on site in cold weather, that difference deserves attention.
Quality Grades A, B, C and D
The letter after the strength number controls impurity limits and toughness. Q235A has the most generous phosphorus and sulfur limits and no impact test requirement; B, C and D tighten the chemistry step by step and add a Charpy V-notch impact test at a progressively lower temperature.
| Quality grade | Phosphorus, max | Sulfur, max | Impact test |
|---|---|---|---|
| Q235A | 0.045 % | 0.050 % | Not required |
| Q235B | 0.045 % | 0.045 % | 27 J at plus 20 degrees Celsius |
| Q235C | 0.040 % | 0.040 % | 27 J at 0 degrees Celsius |
| Q235D | 0.035 % | 0.035 % | 27 J at minus 20 degrees Celsius |
Q235B is the grade most often ordered for welded pipe and general fabrication, because the room-temperature impact test provides a basic guarantee of toughness at very little extra cost. Grades C and D are reserved for low-temperature service, where brittle fracture is the governing design concern.
Q235A and SS400: Commercial Equivalents
Q235A belongs to GB/T 700, while SS400 is defined by JIS G 3101 in Japan. Their yield and tensile strength ranges overlap closely and the two are widely treated as commercial equivalents, but the guarantees differ in an important way. Q235A specifies limits for carbon, manganese, phosphorus and sulfur but does not require a Charpy impact test. SS400 does not fix a chemical composition at all; it guarantees mechanical properties, and the chemistry is agreed between supplier and purchaser. A buyer substituting one for the other should therefore check which guarantee the design actually relies on.
St37 and the Move to EN 10025
St37 is an older German designation from DIN 17100, a standard now largely superseded by EN 10025. St37 is a non-alloy quality structural steel, in other words a mild carbon steel: its properties come from carbon content with only small permitted additions of silicon and manganese, and it contains none of the alloying elements such as chromium, nickel or molybdenum that would make it an alloy steel. Its minimum yield strength of 235 MPa matches Q235, and the tensile strength implied by the designation, 370 MPa minimum, sits inside the Q235 tensile range. In current practice an old drawing that calls for St37 is normally translated to S235JR under EN 10025-2, or to Q235B where the Chinese standard governs.
Pipe Forms and Typical Applications
Electric resistance welded pipe – the common choice for Q235B and Q275 water, gas and structural tube in small and medium diameters.
Spiral submerged arc welded pipe – used for large-diameter water mains, piling and structural pipe in Q235B or Q275.
Seamless pipe – selected where a continuous wall is needed or where the size falls outside the welded range.
Typical duties – building frames, transmission towers, road barriers, greenhouse structures, low-pressure fluid lines and general fabrication.
Frequently Asked Questions
Q: What is the main difference between Q235 and Q275?
The minimum yield strength: 235 MPa for Q235 against 275 MPa for Q275. Q275 also has a higher tensile range and a higher carbon content, so it is stronger but slightly less ductile and a little harder to weld.
Q: Can Q235A be used instead of SS400?
In many general construction applications the two are interchangeable, but the guarantees are not identical, because Q235A controls chemistry without an impact test while SS400 controls mechanical properties with chemistry agreed separately. The specification that governs the project decides.
Q: What does the B in Q235B mean?
It is the quality grade. Q235B has tighter phosphorus and sulfur limits than Q235A and must be impact tested with 27 J minimum Charpy V-notch energy at plus 20 degrees Celsius, which makes it suitable for welded structures at ambient temperature.
Q: Is St37 a carbon steel?
Yes. St37 is classified as a non-alloy quality structural steel, or mild carbon steel, with properties derived mainly from carbon and only small permitted amounts of silicon and manganese.
Q: Which grade should be specified for pipe in cold weather?
For low-temperature service the quality grade matters more than the strength grade, so Q235C or Q235D, tested at 0 degrees or minus 20 degrees Celsius, is normally specified instead of Q235B.
Q: Are the mechanical values the same for every wall thickness?
No. GB/T 700 sets lower minimum yield strength as thickness increases, so the value that applies must be read from the table for the actual thickness being ordered.