Mar 18, 2026 Leave a message

ASTM A671 CJP 115 Class 10 Steel Pipe

1. What is ASTM A671 CJP115 Class 10?

A specification for electric-fusion-welded (EFW) steel pipes designed for low-temperature and high-pressure service.

CJP115: Indicates chemistry (carbon steel) and impact testing at -115°F (-82°C).

Class 10: Hydrostatic test pressure of 1,000 psi (6.9 MPa).

2. Key Material Properties?

Grade: Comparable to API 5L Grade B, but optimized for cryogenic conditions.

Strength: Yield ≥ 35 ksi (240 MPa), Tensile: 60–85 ksi (415–585 MPa).

Impact Test: Charpy V-notch required at -115°F to ensure brittle fracture resistance.

Heat Treatment: Normalized for improved toughness.

3. Typical Applications?

Used in:

LNG pipelines and storage systems.

Arctic oil/gas infrastructure.

Cryogenic process piping (e.g., ethylene, ammonia).

4. Manufacturing Requirements?

Welding: Double-welded seams with 100% radiography inspection.

Chemistry: Low sulfur/phosphorus (max 0.025% each) to prevent cracking.

Testing: Hydrostatic + supplementary impact tests.

5. How does it differ from Class 12?

Class 10 has lower hydrostatic pressure (1,000 psi vs. Class 12's 1,200 psi).

Both share identical CJP115 chemistry/impact requirements.

info-400-400

Send Inquiry