Chemical Composition Requirements
1. Finished Product Analysis of Plates - The manufacturer of the pipe shall analyze each heat of plate. The finished product analysis thus determined shall conform to the requirements of the plate standard for the pipe ordered.
2. Finished Product Analysis of Welds - The manufacturer of the pipe shall conduct finished product analysis on each 500ft (152m) or remainder of finished weld metal. The composition analysis shall conform to the welding process used for the deposited weld metal.
3. Analysis may be performed on mechanical property specimens. The results of the analysis shall be reported to the purchaser.
4. When analyzed as specified in 1 or 2, if one of the specimens does not conform to the specified requirements, double the original number of pipes shall be taken from the same batch and reanalyzed; each of them shall conform to the specified requirements. Unqualified pipes shall be rejected.
Mechanical Property Requirements
1. Tensile Properties:
- Requirements-The transverse tensile properties of welded joints shall meet the minimum requirements for the ultimate tensile strength of the specified plate. In addition, for Classes 3x, 4x, and 5x of Dxx, Hxx, Jxx, and Nxx grades, the transverse tensile properties of the parent material (plate) shall be determined on specimens cut from heat-treated steel pipe. These properties shall meet the mechanical property test requirements of the plate standard.
- Number of Tests-One representative specimen shall be prepared for each batch of finished steel pipe.
- Specimen Location and Orientation-The specimen shall be transverse to the weld at the end of the finished steel pipe and may be cold flattened before final machining to size.
- Test Method-The specimens shall be prepared in accordance with QW-150 of Section 6 of the ASME Furnace and Pressure Vessel Code and the specimens shall be tested at room temperature in accordance with A370 Methods and Definitions.
Transverse Guided Bend Test of Welds:
- Requirement-The bend test is satisfactory if the specimen, after bending, has no cracks or other defects exceeding 1/8 in (3.2 mm) in any direction, except in the weld metal or between the weld and the parent metal. Cracks occurring along the edges of the specimen during the test and measuring less than 1/4 in (6.4 mm) in any direction shall not be considered unsatisfactory.
- Number of Tests-One test (two specimens) shall be made for each lot of finished pipe to represent the lot.
- Location and Direction of Specimens-Two bend specimens shall be taken transverse to the weld at the end of the finished pipe. An alternative method may be agreed upon by the purchaser and the manufacturer to be taken from a test plate of the same material as the pipe, which shall be welded to the end of the cylinder and welded as an extension of the longitudinal seam of the pipe.
- Test Method-The test requirements of A2.5.1.7 of A370 shall be met. For pipe with a wall thickness greater than 3/8 in (9.5 mm) but less than 3/4 in (19.0 mm), the side bend test may be substituted for the face and back bend tests. For wall thickness > 3/4 in, both specimens shall be subjected to the side bend test.