Welding and processing of alloy steel pipes

Why do we need to preheat 150-300℃ before welding?
Preheating can slow down the cooling rate and avoid cold cracks in high carbon equivalent alloy steels (such as P11). The preheating temperature of chromium-molybdenum steel needs to be calculated according to AWS D10.8 specification, for example, 12Cr1MoV steel needs 250℃±20℃. Thermocouple monitoring is required during local heating, and excessive temperature difference will cause excessive welding residual stress.

What are the advantages of laser welding over TIG welding?
The heat affected zone of laser welding is only 0.2-0.5mm, and the deformation is reduced by 70%, which is suitable for thin-walled precision tubes (such as vascular stents). However, the equipment investment is as high as 3 million US dollars, and the groove processing accuracy is required to be ±0.05mm. 6kW fiber laser welders have been widely used in the aerospace field.

Is post-weld heat treatment (PWHT) necessary?
PWHT can eliminate welding residual stress and reduce the hardness to below 22HRC to avoid sulfide stress cracking. For example, ASME B31.3 requires that all alloy steel pipes with P≥0.05% must undergo PWHT. The holding time is calculated according to the wall thickness (1h/inch), and the temperature control accuracy must be within ±14℃.

Tool selection for turning high-hardness alloy steel?

It is recommended to use CBN tools to process materials with HRC>50, and the linear speed is controlled at 80-120m/min. When processing Inconel 718, high-pressure coolant (>70bar) is required to flush and break chips. The tool life is usually only 1/5 of that of carbon steel processing, and the cost accounts for up to 30% of the total processing fee.

How to avoid work hardening during deep hole drilling?

Use a stepped feed strategy (feed per revolution 0.02-0.05mm) with a TiAlN coated drill. The cutting fluid must contain extreme pressure additives (such as sulfurized fats), and the pressure must be>15MPa to ensure chip removal. For example, when drilling 17-4PH stainless steel, a speed exceeding 200rpm will cause a work hardening layer>0.1mm.