Jul 21, 2025 Leave a message

Production process of Q345A steel pipe

Q1: What are the main manufacturing processes of Q345A steel pipe?
The mainstream processes include hot rolling (piercing + rolling), ERW high-frequency welding, spiral welding, etc. Hot-rolled seamless pipes are costly but have strong pressure-bearing capacity, suitable for high-pressure systems; ERW welded pipes have high production efficiency (speed can reach 20-40m/min), suitable for large-scale structural pipes. Thick-walled pipes (>40mm) mostly use JCOE forming process. The CPS (continuous forming welding) technology that has emerged in recent years can increase the welding speed to 60m/min. The cold drawing process is used for precision pipe production, but it will cause work hardening and require subsequent annealing.

Q2: How to choose the heat treatment method for Q345A steel pipes?
Common states are hot-rolled state (AR), normalized state (N), and controlled rolled state (TMCP). Normalizing treatment (880-920℃) can refine the grains and increase the impact toughness by 10-15%. The TMCP process combines strength and weldability by controlling the rolling temperature (final rolling is about 800℃) and cooling rate. For welded pipes, local normalizing (900℃×2min/mm) is often performed in the weld area to eliminate stress. Cold-processed pipes need to be annealed at 650-700℃ to restore plasticity. Tempering treatment (quenching + tempering) can be used when special requirements are met, but the cost increases by more than 30%.

Q3: How to control the dimensional accuracy of Q345A steel pipes?
Hot-rolled seamless pipes implement GB/T 17395 C-level accuracy (outer diameter ±0.75%, wall thickness ±10%); cold-drawn pipes can reach D-level (±0.3%). The ovality of the welded pipe should be ≤1.5%D, and the straightness should be ≤1.5mm/m. Precision hydraulic cylinders have higher requirements (such as GB/T 8713 specifies a wall thickness tolerance of ±5%). Laser diameter gauges (accuracy ±0.02mm) and ultrasonic thickness gauges are used for online detection during production. For large diameter pipes (>508mm), the effects of thermal expansion and contraction need to be considered (the diameter changes by about 0.012% for every 10℃ change in temperature).

Q4: What are the surface treatment technologies for Q345A steel pipes?
Anti-corrosion treatment includes hot-dip galvanizing (zinc layer ≥80μm), epoxy powder spraying (200-300μm), PE/PP coating, etc. Before galvanizing, pickling (HCl concentration 15-20%) is required to remove the oxide scale and zinc immersion at 430-450℃. Sandblasting (Sa2.5 grade) can improve the adhesion of the coating (≥10MPa). Weathering steel can form a protective rust layer through Cu-P-Cr alloying. Special environments (such as offshore platforms) require "galvanizing + coating" double protection, and the design life can reach 30 years. Cement mortar lining or polyurethane coating is commonly used for inner wall corrosion protection.

Q5: What are the key points of the welding process of Q345A steel pipes?
It is recommended to use ER50-6 welding wire (GB/T 8110), preheating temperature 100-150℃ (for plate thickness >25mm). Welding heat input is controlled at 15-35kJ/cm, and interlayer temperature ≤250℃. For thick-walled pipes (>40mm), post-weld dehydrogenation treatment (250℃×2h) is required. Submerged arc welding (SAW) has the highest efficiency (deposition rate ≥8kg/h), and gas shielded welding (GMAW) is more suitable for on-site installation. Important welds should be tested by 100% UT, and the acceptance standard is in accordance with the requirements of Level II of JB/T 4730.3. Note that the carbon equivalent of Q345A is about 0.38%, and the tendency of cold cracking is greater than that of Q345D.

info-259-194info-259-194info-232-217

Send Inquiry