1. Q: What is a "laminated pipe defect"?
A: An internal flaw where layers of metal are separated or not fully bonded, often originating from the ingot. It can seriously weaken the pipe wall.
2. Q: Why are radiography (RT) and ultrasonic testing (UT) performed on pipes?
A: RT uses X-rays or gamma rays to detect internal defects like voids, inclusions, or lack of weld penetration. UT uses sound waves to detect subsurface flaws and measure wall thickness.
3. Q: What causes graphitization in carbon steel?
A: Prolonged exposure to temperatures above 425°C (800°F) can cause the carbon in the steel to transform into free graphite nodules, weakening the material and making it brittle.
4. Q: What is a "coupon" in pipe context?
A: A sample piece of the pipe material, often taken from the pipe end or a test plate, used for mechanical or chemical testing to verify properties.
5. Q: What is the primary purpose of pipe coating (e.g., FBE, 3LPE)?
A: To provide external corrosion protection when the pipe is buried or exposed to corrosive environments. Common coatings include Fusion-Bonded Epoxy (FBE) and 3-Layer Polyethylene (3LPE).