What is the yield strength of Q235B carbon steel pipe? How to test?
The yield strength of Q235B is ≥235MPa (when the thickness is ≤16mm), and the test is based on GB/T 228.1 standard. The specimen is slowly loaded on the tensile machine, and the stress-strain curve is recorded. The stress corresponding to the yield platform is the yield strength. This grade is widely used in building structures because of its good plasticity and weldability. As the thickness increases, the yield strength decreases slightly (such as 225MPa when the thickness is 20mm).
Is the tensile strength of carbon steel pipe related to wall thickness?
The tensile strength mainly depends on the material (such as Q345 is higher than Q235), and has no direct relationship with the wall thickness. However, due to the slow cooling rate of thick-walled pipes, the grains may be coarse and the strength is slightly lower. The strength of thin-walled pipes is improved after cold working (such as cold-drawn pipes). When designing, the grade should be selected according to standards such as GB/T 8163, rather than relying solely on wall thickness. Extremely thin walls (such as D/t>50) may cause local buckling failure.
Why do carbon steel pipes need to be marked with elongation indicators?
Elongation (such as Q235's δ₅≥26%) reflects the ability of plastic deformation. High elongation materials are not easy to break when impacted or overloaded. When the pipeline needs to be bent or expanded during installation, low elongation is prone to cracking. Elongation is measured by tensile testing, and the gauge length is usually 5 times the diameter (δ₅). Higher elongation is required in cold areas to prevent low-temperature brittle cracking. Standards such as ASTM A106 have grading requirements for elongation.
Will carbon steel pipes become brittle at low temperatures? How to improve it?
Cold brittle fracture may occur in carbon steel pipes below -20℃, especially when the sulfur and phosphorus content is high. Improvement measures include: using calm steel (such as Q235D containing nickel), controlling sulfur and phosphorus content (≤0.025%), or performing normalizing treatment to refine grains. Low-carbon equivalent steel (such as API 5L Gr.B) is commonly used in Arctic pipelines. Charpy V-notch impact test can evaluate low-temperature toughness.
What is the fatigue strength of carbon steel pipes? What factors affect it?
Fatigue strength is usually 40-50% of tensile strength (such as about 150MPa for Q235). Influencing factors include: surface defects (scratches, rust), stress concentration (unpolished welds), and cyclic load frequency. Shot peening can increase surface compressive stress and extend life. Under high-frequency fatigue (such as 10⁶ cycles), carbon steel pipes need to be tested by SN curve. Corrosive environment will greatly reduce fatigue strength.