What steels are commonly used for spiral submerged arc welded pipes?
Low carbon steel (such as Q235B) is used for low-pressure pipelines, and X series (X42–X80) is used for high strength requirements. Low temperature resistant steel (such as L245) is suitable for cold regions. Stainless steel or alloy steel is used in corrosive environments. The material must comply with API 5L or GB/T 9711 standards. Material selection requires a comprehensive consideration of strength, toughness and weldability.
How to evaluate the low temperature toughness of pipes?
The impact energy below -20°C is measured by the Charpy impact test. The drop weight tear test (DWTT) evaluates the brittle fracture tendency. The material must meet the ductile-brittle transition requirements at a specific temperature. Low temperature steels need to add alloying elements such as nickel and vanadium. Arctic pipelines require toughness at -60°C.
Why do we need to control sulfur and phosphorus content?
Sulfur causes hot brittleness and is prone to cracking during welding. Phosphorus increases cold brittleness and reduces low temperature toughness. Both deteriorate the ductility of the weld metal. API standards stipulate that sulfur ≤ 0.03% and phosphorus ≤ 0.03%. The use of an off-furnace refining process can effectively reduce impurities.
How to choose an anti-corrosion coating?
Three-layer PE (polyethylene) coating is suitable for most soil environments. Fusion bonded epoxy powder (FBE) is resistant to high temperatures and has strong adhesion. Polyurethane coating is used for wear resistance. Submarine pipelines need to be equipped with cathodic protection. Coating selection needs to consider cost, construction conditions and life cycle.
How to improve the pipeline's resistance to hydrogen-induced cracking?
Choose low-hardness, high-purity steel. Add copper and chromium elements to inhibit hydrogen sulfide corrosion. Control welding heat input to reduce sensitive tissues. Post-weld heat treatment eliminates residual stress. Need to pass NACE TM0284 standard test.