The construction quality of the anti-corrosion layer in the spiral pipe and the quality of the anti-corrosion layer in the cement mortar should comply with the following rules.
① The width of the crack shall not be greater than 0.8 mm, the longitudinal length along the pipeline shall not be greater than the circumference of the pipeline, and shall not be greater than 2.0 m.

② The allowable deviation of the thickness of the anti-corrosion layer and the depth of surface defects such as pitting and hollows should comply with the regulations, and the defect area should not be larger than 5 cm2 at each location.
③ The flatness requirement is to use a 300 mm long ruler against the pipe wall along the longitudinal axis of the pipeline. The gap between the surface of the anti-corrosion layer and the ruler should be less than 2 mm.

④The hollow area shall not exceed 2 places per 1 m2, and each place shall not be larger than 100 cm2.
Of course, there are many ways to use the internal method of spiral pipes. Cement mortar is only one method, and there are other methods such as the use of anti-corrosion coatings.