Introduction to Inconel 718 Tubing & Pipe

Inconel 718 is a high-strength, nickel-chromium superalloy known for its exceptional performance in extreme environments. It is precipitation-hardenable, meaning it can be heat-treated to achieve very high strength. Its key characteristics are excellent resistance to oxidation and corrosion, high yield and tensile strength, and most notably, its ability to retain these properties at high temperatures (up to ~1300°F / 700°C). It also exhibits good weldability.

Primary Applications:

Aerospace: Jet engine components, liquid rocket parts, casings, rings.

Oil & Gas: High-pressure, high-temperature (HPHT) well components, downhole instrumentation housings, packers, subsurface safety valves.

Power Generation: Gas turbine parts, heat exchangers, nuclear reactors.

Chemical Processing: Equipment exposed to highly corrosive media.


Key Product Parameters & Properties

1. Chemical Composition (ASTM B637)

The following table outlines the standard chemical composition range for Inconel 718.

 
 
Element Content (%) Element Content (%)
Nickel (Ni) 50.0 - 55.0 Aluminum (Al) 0.20 - 0.80
Chromium (Cr) 17.0 - 21.0 Titanium (Ti) 0.65 - 1.15
Iron (Fe) Balance Cobalt (Co) ≤ 1.00
Niobium (Nb) 4.75 - 5.50 Copper (Cu) ≤ 0.30
Molybdenum (Mo) 2.80 - 3.30 Carbon (C) ≤ 0.08
Manganese (Mn) ≤ 0.35 Boron (B) ≤ 0.006
Silicon (Si) ≤ 0.35 Sulfur (S) ≤ 0.015

The combination of Niobium (Nb) and Molybdenum (Mo) is primarily responsible for the alloy's exceptional strength after precipitation hardening.

2. Mechanical Properties

Mechanical properties are highly dependent on the heat treatment condition. The standard heat treatment for maximum strength is Solution Annealed + Aged.

Typical Room Temperature Mechanical Properties (ASTM B637 - Bar & Forging, indicative for tubing)

 
 
Condition Tensile Strength Yield Strength (0.2% Offset) Elongation (%)
Annealed 125 ksi (862 MPa) 95 ksi (655 MPa) 25%
Solution Treated & Aged 185 ksi (1275 MPa) 150 ksi (1035 MPa) 20%

Note: Properties for thin-walled tubing may vary. Specific values should be confirmed with the manufacturer based on the product form and size.

3. Physical Properties

 
 
Property Value
Density 0.297 lb/in³ (8.19 g/cm³)
Melting Range 2300-2460°F (1260-1350°C)
Thermal Expansion Coefficient 7.4 x 10⁻⁶ /°F (13.3 x 10⁻⁶ /K) @ 70-1200°F
Thermal Conductivity 70 Btu·in/(hr·ft²·°F) (10.1 W/m·K) @ 212°F (100°C)
Modulus of Elasticity 29.1 x 10⁶ psi (201 GPa)

Product Specifications & Standards Table

Inconel 718 tubing and pipe are produced to various international standards, which define the chemical, mechanical, and dimensional requirements.

 
 
Product Form Standard Number Standard Title (Scope)
Seamless Pipe & Tube ASTM B829 Standard Specification for Seamless Nickel and Nickel Alloy Condenser and Heat-Exchanger Tubes
Seamless Pipe ASTM B516 Standard Specification for Welded Nickel and Nickel-Alloy Economizer, Superheater, Heat-Exchanger, and Condenser Tubes
Welded Tube ASTM B760 Standard Specification for Welded Round Nickel-Alloy Tubes for General Purpose Applications
Bar & Forging (for machined parts) ASTM B637 Standard Specification for Precipitation-Hardening Nickel Alloy Bars, Forgings, and Forging Stock for High-Temperature Service
Aerospace AMS 5596 Nickel Alloy, Corrosion and Heat-Resistant, Sheet, Strip, and Plate 52.5Ni - 19Cr - 3.0Mo - 5.1Cb - 0.90Ti - 0.50Al - 18.5Fe
Aerospace AMS 5662 Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 52.5Ni - 19Cr - 3.0Mo - 5.1Cb - 0.90Ti - 0.50Al - 18.5Fe Solution Heat Treated, Precipitation Hardenable

Key Advantages Summary

High-Temperature Strength: Excellent creep rupture and tensile strength up to 1300°F (700°C).

Precipitation Hardenable: Can be heat-treated to achieve very high strength levels, surpassing many other nickel alloys in its useful temperature range.

Oxidation & Corrosion Resistance: Outstanding resistance to oxidation and a wide range of corrosive environments, including sour gas (H₂S).

Good Fabricability: Can be welded and fabricated using standard techniques, though post-weld heat treatment is often recommended.

Phase Stability: The addition of Niobium prevents the formation of deleterious phases during prolonged exposure to high temperatures, which can embrittle other alloys.

For specific projects, it is crucial to consult with materials engineers and the tubing manufacturer to select the correct heat treatment, size, and specification to meet the application's precise mechanical, corrosion, and temperature requirements.