1. Material Composition & Key Properties
Q: What defines the chemical/mechanical properties of E275 steel?
A:
Chemical (wt%):
C: ≤0.20 | Mn: 0.50–1.40 | P: ≤0.025 | S: ≤0.020.
Mechanical:
Yield Strength (σᵧ): ≥275 MPa | Tensile (σₜ): 410–560 MPa.
Elongation (A₅): ≥22% | Hardness: ≤160 HB.
Note: E275 is a non-alloy steel with better strength than E235 but similar weldability (Ceq ≤0.40).
2. Manufacturing & Standards
Q: How are these tubes produced and certified?
A:
Process: Seamless (hot/cold-finished) or welded (ERW/SAW).
Heat Treatment: Normalized (EN 10297-1 §6.2) or stress-relieved.
Key Standard: EN 10297-1 (Mechanical/engineering applications).
3. Dimensional Tolerances
Q: What are the allowed dimensional deviations?
A:
| Parameter | Tolerance |
|---|---|
| OD (D) | ±1.0% (min ±0.5 mm) |
| Wall Thickness | ±10% (min ±0.3 mm) |
| Straightness | ≤1.5 mm/m (cold-drawn: ≤1.0) |
4. Applications & Limitations
Q: Where is E275 typically used?
A:
Structural: Crane booms, conveyor rollers (seamless).
Fluid Systems: Low-pressure hydraulics (welded, if leak-tested).
Avoid: High-temperature (>400°C) or acidic environments.
5. Quality Validation
Q: How is quality assured?
A:
Tests: Tensile (EN ISO 6892-1), hardness (EN ISO 6506-1).
Certification: EN 10204 3.1/3.2 | PED 2014/68/EU for pressure use.