Both ST52 and S355 are hollow tube materials for structures, but they belong to different standard systems: ST52 is derived from the German DIN standard (such as the St52-3 series), and S355 is derived from the European EN standard (such as S355J2 or S355B). There are significant differences between the two in terms of strength, chemical composition and application characteristics. The following is a core comparison:

 

1. Standards and material characteristics

index‌ ‌ST52 hollow section‌ ‌S355 hollow section‌
‌Standard system‌ DIN EN
‌Yield Strength‌ ≥355MPa(thickness ≤16mm),Decreases with increasing thickness ≥355MPa (nominal value), higher stability‌
Tensile Strength‌ 490–630MPa ‌ 470–630MPa(like Q355B)‌
Chemical Composition‌ Carbon content ≤ 0.20%, phosphorus and sulfur impurities are less controlled Optimized alloying elements (e.g. higher manganese content) and tighter impurity control

S355 hollow section

2. Differences in performance and application

  • Low temperature toughness ‌:

ST52: Good toughness, but low temperature performance (such as 0℃ impact energy ≥ 23J) is weaker than S355, suitable for normal temperature environment ‌.
S355: Better low temperature toughness (such as S355J2), suitable for structures in cold areas, and stronger impact resistance ‌.

  • ‌ Welding and processing ‌:

ST52: Excellent weldability, no need for complex preheating process, suitable for general structural parts.
S355: Better welding adaptability, but temperature control is required to prevent cracking, suitable for high-precision welding scenarios ‌.

  • ‌ Application scenarios ‌:

ST52: Mainly used for medium-sized structural parts, such as mechanical brackets, vehicle chassis or low-pressure pipelines.
S355: Preferred for heavy load or dynamic load environments such as high-rise buildings, bridges, wind power towers ‌.

 

3. Summary and suggestions

Focus on selection:

Load requirements ‌: S355 is preferred for heavy load or low temperature environments (cost-effectiveness is better than higher strength materials) ‌.
‌Cost factor‌: ST52 is cheaper, but S355 has a longer lifespan under harsh conditions ‌

 