Jul 24, 2025 Leave a message

What is the difference between C250 and C350 hollow section

C250 and C350 hollow tubes are both cold-formed structural hollow profiles under the Australian Standard (AS). The core differences are reflected in strength, composition and applicable scenarios. The following is a specific comparison:

1. Core performance differences

index‌ ‌C250 Hollow Section‌ ‌C350Hollow Section‌
‌Yield Strength‌ ≥250MPa ‌ ≥350MPa ‌
‌Tensile Strength‌ ≥300MPa(Reference Low Carbon Steel)‌ ≥450MPa ‌
‌Material composition‌ Low carbon steel (carbon content 0.22%~0.29%) Medium carbon steel (carbon content 0.32%~0.40%)
‌Toughness performance‌ Excellent plasticity, elongation ≥ 24% ‌ Higher hardness and stronger resistance to deformation

C250 hollow section

2. Comparison of processing and durability

Welding and cold processing:
C250: Low carbon properties make it easier to weld and cold bend, without complex preheating process;
C350: High carbon content, welding requires preheating to prevent cracking, and cold processing is more difficult.
Weather resistance:
C350 adds chromium, nickel and other elements, and its corrosion resistance is better than C250, which is more suitable for harsh outdoor environments;
Both require surface anti-corrosion treatment (such as coating) to extend life 

 

3. Applications

T‌ype A‌pplications
‌C250‌ Light duty shelves, interior decoration frames, low pressure fluid pipelines ‌
‌C350‌ High-rise building pillars, heavy machinery frames, vehicle load-bearing components

 

Send Inquiry