Jul 25, 2025 Leave a message

1018 vs 1045 Steel: Composition, Properties and Application Differences

What AISI 1018 and 1045 Steel Are

AISI 1018 and AISI 1045 are plain carbon steels described by the SAE four-digit designation system, in which the last two digits indicate the nominal carbon content in hundredths of a percent. Grade 1018 is a low-carbon steel with about 0.18% carbon; grade 1045 is a medium-carbon steel with about 0.45% carbon. Both are produced as hot rolled bar, cold drawn bar, seamless tube and forged shapes, and both are widely exported from China in metric and imperial sizes.

The designation alone tells the buyer the single most important fact about the grade: 1018 is selected for formability, weldability and consistent machined finish, while 1045 is selected because it can be quenched and tempered to a much higher strength level. Neither grade contains deliberate alloying additions beyond manganese, so their properties come from carbon content and from the way the mill or the end user processes them.

Chemical Composition and Mechanical Properties

The composition ranges below follow the standard AISI/SAE chemistry for the two grades. Mechanical values are typical figures for the common delivery conditions and are quoted to show the relative behaviour of the two materials rather than to replace a mill certificate.

Item AISI 1018 AISI 1045
Carbon 0.15-0.20% 0.43-0.50%
Manganese 0.60-0.90% 0.60-0.90%
Phosphorus / sulphur 0.040% max each 0.040% max each
Typical hardness, hot rolled about 126 HB about 163-200 HB
Typical tensile strength about 440 MPa in the cold drawn condition about 565-600 MPa hot rolled or normalised
Typical yield strength about 370 MPa cold drawn about 310 MPa hot rolled, rising after quenching and tempering
Weldability Excellent, no preheat normally required Fair, preheat and controlled cooling usually required
Response to heat treatment Limited; case hardening only Strong; through hardening and induction hardening
Equivalent European grades C15 / 1.1141 C45 / 1.1191, GB/T 699 grade 45

Heat Treatment, Machinability and Welding

1018 cannot be strengthened by quenching in any useful way because its carbon content is too low. It can be case carburised to give a hard, wear-resistant skin over a tough core, and it is normally supplied cold drawn to a controlled hardness so that it machines cleanly on automatic lathes. Chips break easily, tool wear is low and dimensional stability after machining is good, which is why 1018 is a default choice for high-volume turned parts.

1045 responds strongly to heat treatment. Water or polymer quenching followed by tempering produces a wide range of strength and toughness combinations, and induction or flame hardening can localise hardness on wear surfaces such as shaft journals. In the as-supplied hot rolled condition 1045 is harder and less ductile than 1018, so it demands lower cutting speeds, rigid tooling and more attention to chip control. It is also more crack sensitive: welding 1045 calls for preheat in the region of 150-250 degrees Celsius, controlled interpass temperature and slow cooling, while 1018 can be welded with ordinary carbon steel procedures using a filler that matches the base strength.

Typical Applications

1018: shafts, pins, spindles, studs, tie rods, hydraulic fittings, brackets, fixture plates, low-stress gear blanks and general machinery parts where good finish and weldability matter more than strength.

1045: axles, drive shafts, gears, sprockets, crankshafts, couplings, bolts and studs, plough and harrow parts, and any component that will be quenched and tempered or induction hardened.

How to Choose Between the Two Grades

Start from the required strength and the manufacturing route. If the part is produced mainly by machining and welding and does not need a hardness above roughly 200 HB, 1018 gives the lowest total cost because it machines quickly and needs no thermal treatment. If the part must carry high loads, resist wear or be hardened after machining, 1045 is the economical choice because it develops the required properties through heat treatment rather than through alloying. Where a design calls for both a hard surface and a tough core, a case carburised 1018 part is often preferred over a through hardened 1045 part because the core remains ductile. Where distortion after heat treatment must be minimised, confirm the hardenability and the tempering cycle with the mill before committing to 1045, and consider a controlled-atmosphere anneal before machining.

Both grades are ordered by chemistry and by delivery condition, so the purchase specification should always state the condition, the tolerance class and the surface finish in addition to the grade name.

FAQ

Q: Is 1045 stronger than 1018?
In the as-supplied condition 1045 is stronger, with roughly 565 to 600 MPa tensile strength against about 440 MPa for cold drawn 1018. After quenching and tempering, 1045 can reach several times the strength of 1018, which cannot be hardened by quenching at all.

Q: Can 1018 be hardened?
1018 cannot be through hardened because its carbon content is too low. It can be case carburised or carbonitrided to produce a hard surface layer while the core stays soft and tough.

Q: Is 1045 weldable?
1045 is weldable but requires care. Preheat of roughly 150 to 250 degrees Celsius, controlled heat input, and slow cooling after welding are used to avoid a hard, crack-prone heat affected zone. A post-weld tempering treatment is common for critical joints.

Q: Which grade machines better?
1018 machines better in the cold drawn condition because it is softer and produces well-broken chips. 1045 machines well in the annealed or cold drawn condition but needs lower speeds and feeds, especially after normalising.

Q: What is the Chinese equivalent of 1045 steel?
GB/T 699 grade 45 steel is the closest Chinese equivalent, and it is the grade normally quoted for export orders that specify a 0.45% carbon bar. For 1018 the nearest common equivalents are C15 and GB/T 699 grades 15 or 20.

Q: Are 1018 and 1045 available as tube and pipe as well as bar?
Yes. Both chemistries are produced as seamless tube and as cold drawn tube, and they can be supplied as welded and drawn tubing where a smooth bore and tight wall tolerance are needed.

Send Inquiry