Nov 26, 2025 Leave a message

ASTM A691 1-1/4Cr EFW Alloy Steel Pipe: Specification and Properties

What Is ASTM A691 1-1/4Cr Pipe?

ASTM A691 is the standard specification for electric-fusion-welded (EFW) chromium-molybdenum alloy steel pipe intended for high-temperature, high-pressure service. The 1-1/4Cr designation identifies the grade: a low-alloy steel containing nominally 1.25% chromium combined with molybdenum, the classic Cr-Mo pairing used for elevated-temperature strength, creep resistance and oxidation resistance.

Because the pipe is formed from plate or sheet, joined with filler metal by an electric-fusion welding process and finished with a longitudinal seam, it is normally specified where large diameters and heavy walls are required and where a seamless mill cannot supply the size. The specification covers chemistry, heat treatment, tensile requirements, weld quality, inspection and testing of the finished pipe.

A691 pipe is ordered as a grade and class combination. The grade fixes the chemical composition of the base metal and the filler metal, while the class fixes the minimum tensile strength level and the heat-treatment condition in which the pipe is supplied. Both parts of the designation must be stated on the purchase order.

Chemical Composition and Mechanical Requirements

The 1-1/4Cr grade is a chromium-molybdenum steel of the same family as the ferritic alloy grades used for high-temperature piping. The alloying ranges below are the ones that govern the grade; carbon is kept deliberately low for weldability, and residual elements are restricted to protect toughness.

Element Typical requirement for 1-1/4Cr Purpose
Cr 1.00-1.50% Oxidation and scaling resistance at temperature
Mo 0.44-0.65% Creep strength and elevated-temperature tensile strength
C Controlled low-carbon range Weldability and ductility of the weld heat-affected zone
Mn, Si Specified per the standard Deoxidation and strength balance
P, S Restricted Toughness, weld soundness

The filler metal must deposit a weld that matches the Cr-Mo chemistry of the base metal, and the deposited weld metal must meet the mechanical property requirements of ASTM A691 for the ordered grade and class. Tensile strength, yield strength and elongation limits rise with the class number, so the mechanical values must always be taken from the standard's property table for the exact grade and class on the order.

Manufacturing Route: Electric-Fusion-Welded Construction

Plate is cut, edge-prepared, rolled or pressed to a cylindrical shell and joined by a longitudinal seam with filler metal added. Double-sided submerged arc welding is common for heavy walls. The sequence that matters for final quality is:

Plate verification against the ordered grade chemistry.

Fit-up and alignment control so that offset stays within the dimensional limits of the standard.

Weld parameter control: heat input, interpass temperature and flux condition all influence toughness.

Heat treatment of the finished pipe in the condition required by the class - either stress relieving or normalising and tempering.

Non-destructive examination of the longitudinal seam and a hydrostatic test of each length.

Dimensional inspection, marking and issuance of the material test certificate.

Post-weld heat treatment is not cosmetic. On 1-1/4Cr material it restores ductility and toughness in the weld heat-affected zone and relaxes residual stress, so the heat-treatment record for each lot should be reviewed together with the mechanical test results.

Applications in High-Temperature Service

1-1/4Cr pipe is widely used as elevated-temperature pressure piping where carbon steel has run out of creep strength but a more highly alloyed grade is not yet justified on cost:

Refinery process piping - hydrotreater, reformer and hydrocracker circuits.

Power generation - steam and hot reheat lines, boiler outlet piping and steam headers.

Chemical and petrochemical plants - reactors, heat exchangers and transfer lines.

Furnace and reformer piping operating continuously in the creep range.

Because the material holds strength at temperature and forms a protective oxide scale, it is often chosen for lines that see steady thermal load rather than for lines that cycle heavily at low temperature.

Ordering, Welding and Inspection Notes

For field and shop welding of 1-1/4Cr pipe, preheating in the range normally specified for low-alloy Cr-Mo steel (about 150-200 degrees C) is standard practice, followed by controlled interpass temperature, matching Cr-Mo filler metal, and post-weld heat treatment on completion. Rapid cooling of a heavy-section weld without heat treatment is a common cause of hard, crack-sensitive heat-affected zones.

Points worth checking on delivery: the pipe grade and class on the certificate against the purchase order; chemistry and tensile results for each heat and each lot; the heat-treatment record; the welding procedure specification and procedure qualification record for the longitudinal seam; radiographic or ultrasonic results for the seam; hydrostatic test pressure and duration; and dimensional tolerances at the ends.

FAQ

Q: What does 1-1/4Cr mean in ASTM A691?
It is the grade designation: the steel contains nominally 1.25% chromium together with molybdenum, giving the pipe its elevated-temperature strength and oxidation resistance.

Q: How does A691 differ from a seamless alloy pipe specification?
A691 covers pipe made by electric-fusion welding from plate with filler metal added, so it suits large diameters and heavy walls. Seamless specifications cover pipe produced without a longitudinal weld and are generally used for smaller diameters.

Q: What does the class number tell a buyer?
The class sets the minimum tensile strength level and the heat-treated condition of the finished pipe. Grade and class must both be quoted, because the same chemistry can be supplied at different strength levels.

Q: Is post-weld heat treatment mandatory?
For low-alloy Cr-Mo material in the thicknesses typical of this grade, heat treatment is normally specified to temper the weld heat-affected zone and relieve residual stress. The exact requirement follows the applicable construction code and the ordered class.

Q: Where is 1-1/4Cr pipe most often used?
In refinery and petrochemical process piping and in power plant steam systems, wherever service temperature exceeds the practical limit of carbon steel but does not require a higher-alloy grade.

Q: What should be verified on the mill certificate?
Grade and class, heat number, chemical analysis, tensile and yield results, heat-treatment condition, weld examination results and the hydrostatic test record for each length.

Send Inquiry