1. **Difference between A671 and A672:**
* **ASTM A671:** Covers **arc-welded** steel pipe for atmospheric and lower temperatures. The pipe is fabricated from plate or sheet and welded with filler metal added. It's primarily used for low-temperature service down to -50°F (-45°C) or colder, depending on the grade/class.
* **ASTM A672:** Covers **electric-fusion-welded** steel pipe for high-pressure service at **moderate** temperatures. The pipe is fabricated from plate or sheet and welded using processes (like SAW or ERW variations) that often melt the base metal without adding filler metal. It's designed for higher pressures but is restricted to service temperatures above +650°F (+340°C).

2. **ASTM A672 Grade C65:**
* ASTM A672 Grade C65 refers to a specific classification within the A672 standard for EFW pipe.
* "C" indicates the pipe is made from **carbon steel**.
* "65" indicates the **minimum specified yield strength** is 65,000 psi (448 MPa).
* This grade requires **hydrostatic testing** and is suitable for **high-pressure** service at **moderate temperatures** (above +650°F / +340°C).

3. **ASTM A671 Grade:**
* The term "grade" in ASTM A671 refers to the **type of steel** used to fabricate the welded pipe. Common grades include:
* **CA, CB, CC:** Carbon steel grades with increasing levels of Charpy V-notch impact toughness (tested at lower temperatures). CC offers the highest low-temperature toughness.
* **CD, CE:** Carbon-manganese steel grades, also with varying toughness levels.
* Each grade is further subdivided into **Classes** (e.g., Class 12, 22, 32, 42, 52, 62, 72) which define the required **minimum Charpy V-notch impact energy absorption** at a specified test temperature. Higher class numbers generally require higher impact energy at colder temperatures.

4. **Difference between ASTM A671 and ASTM A333:**
* **ASTM A671:** Covers **welded** pipe fabricated from plate/sheet. It's specifically designed for **low-temperature** service (down to -325°F / -198°C for Grade CC Class 1). Its primary focus is toughness at cryogenic or very low temperatures.
* **ASTM A333:** Covers **seamless and welded** pipe. While it also covers low-temperature service (Grades 1, 6, 7, 3, 4, 8, 9, 10, 11), its temperature range is generally **not as extreme** as the coldest grades of A671 (common Grade 6 is for -50°F / -45°C). A333 covers a wider range of materials (carbon steel, alloy steel, nickel alloy) and applications beyond just extreme cryogenics, including moderate low-temp service.

5. **What ASTM means in pipes:**
* **ASTM** stands for **ASTM International**, formerly known as the American Society for Testing and Materials.
* In the context of pipes (like ASTM A671, A672, A333), "ASTM" signifies that the pipe is manufactured according to a specific technical standard published by ASTM International.
* These standards define critical requirements such as:
* Permitted materials (chemical composition, steel grade)
* Manufacturing process (seamless, welded method)
* Mechanical properties (yield strength, tensile strength, toughness/impact testing)
* Testing requirements (hydrostatic, non-destructive examination)
* Dimensions and tolerances
* Marking and certification
* Using ASTM standards ensures consistency, reliability, and fitness-for-purpose of the pipe material. Engineers and inspectors rely on these specifications for design and verification.