Jul 31, 2025 Leave a message

ASTM A519 Grade 4621 Nickel-Molybdenum Seamless Mechanical Tubing

What ASTM A519 Grade 4621 Tubing Is

ASTM A519 grade 4621 is a low-carbon nickel-molybdenum alloy steel supplied as seamless mechanical tubing and registered under the UNS number G46210. It is an established low-temperature and pressure-component grade: nickel at 1.80–2.20% raises toughness and hardenability while suppressing the ductile-to-brittle transition, and molybdenum at 0.25–0.35% adds hardenability and limits temper embrittlement.

Because the grade hardens deeply but retains toughness after tempering, it is used where a tubular component has to carry pressure or mechanical load in cold conditions, or where the design must tolerate impact loading without brittle failure. It is normally supplied in the quenched and tempered condition when mechanical properties are specified.

Chemical Composition

Element ASTM A519 grade 4621
Carbon 0.18–0.23%
Manganese 0.45–0.65%
Silicon 0.15–0.35%
Nickel 1.80–2.20%
Molybdenum 0.25–0.35%
Phosphorus 0.035% max
Sulphur 0.040% max

Unlike the carburizing grades, 4621 is intended to be used through its section rather than with a hardened case. The carbon level is high enough to respond to quenching and tempering, the absence of chromium leaves a simple nickel-molybdenum system with good weldability relative to chromium-bearing alloys, and the combination is well suited to components that must be joined by welding and then heat treated.

Mechanical Properties and Low-Temperature Behaviour

ASTM A519 tabulates minimum tensile strength, yield strength and elongation for each grade and delivery condition, so the figures quoted for a 4621 order depend on whether the tube is supplied hot finished, cold drawn or heat treated. In the quenched and tempered condition the grade is typically selected for a strength range in which impact toughness at low service temperature remains the governing property, so orders for cold-service components normally include a Charpy impact test at an agreed test temperature.

Impact test temperature, energy absorption and specimen orientation should all be stated on the order, because toughness values are meaningless without them. Where the component is welded, the test is frequently applied to the weld and heat affected zone as well as to the parent tube.

Heat Treatment and Welding

The normal route for a tubular component is to machine or form in the annealed condition, weld if required, then austenitize, quench in oil and temper to the specified strength and toughness. Oil quenching suits the section sizes typical of mechanical tubing and limits distortion compared with a water quench. Tempering temperature is selected to balance strength against low-temperature toughness, and the cooling rate after tempering should be controlled on heavy sections to avoid temper embrittlement.

The grade is more weldable than the chromium-bearing carburizing and through-hardening alloys, but welding still requires a qualified procedure: a low-hydrogen consumable, a modest preheat on thicker sections and a controlled interpass temperature. Welded components should be heat treated after welding if the design requires the parent properties to be restored.

Typical Applications

Pressure-bearing sleeves, housings and cylinders for low-temperature service

Support structures and connection components for cryogenic storage and transport equipment

Hydraulic and pneumatic cylinders for cold-climate machinery

Heavy-duty shafts and drive components in cold-region mining and construction equipment

Structural tubular members requiring toughness under impact loading

FAQ

Q: What is UNS G46210?
It is the unified numbering system identifier for the 4621 nickel-molybdenum chemistry listed among the standard grades of ASTM A519. The UNS number identifies the composition, while ASTM A519 sets the requirements for the tubular product.

Q: What gives 4621 its low-temperature toughness?
The nickel content of 1.80–2.20% improves toughness and lowers the ductile-to-brittle transition temperature, while molybdenum adds hardenability and limits temper embrittlement. The combination allows the grade to remain ductile at low service temperatures.

Q: How does 4621 compare with 4620 tubing?
Both are nickel-molybdenum grades. Grade 4621 carries higher nickel and molybdenum ranges than 4620, which improves hardenability and low-temperature toughness, so it is preferred for colder service or heavier sections.

Q: Can 4621 tubing be welded?
Yes, with a qualified procedure. The simple nickel-molybdenum composition gives better weldability than chromium-bearing alloys, but a low-hydrogen consumable, a modest preheat on thick sections and post-weld heat treatment where properties must be restored are still required.

Q: Should impact testing be specified for grade 4621?
Yes, whenever the component serves in cold conditions. State the test temperature, the minimum absorbed energy and the specimen orientation, and apply the test to the welded joint as well as to the parent tube where welding is used.

Q: How should grade 4621 tubing be ordered?
State the grade and UNS number, the delivery condition, the finished size, the required strength and impact properties with their test temperature, and the examination requirements. Because ASTM A519 properties depend on delivery condition, that condition must be stated explicitly.

Send Inquiry