ASTM A500/A500M Cold-Formed Welded and Seamless Carbon Steel Structural Tubing
A500 steel pipe is a type of carbon steel structural tubing produced in accordance with the ASTM A500 standard. This standard specifies the requirements for welded or seamless carbon steel round, square, and rectangular tubing, primarily intended for structural applications.
Production Standards
The ASTM A500 standard specifies the specifications for cold-formed welded and seamless carbon steel structural tubing in round, square, and rectangular shapes.
It covers multiple grades, with Grade A, B, C, and D being common, each having different requirements for tensile strength, yield point, and other mechanical properties to meet the needs of various engineering applications.
Characteristics
High Strength:
A500 steel tubing has high tensile and yield strengths, enabling it to withstand large loads and deformations without failure, making it suitable for building structures, bridges, and other load-bearing applications.
Good Toughness:
Exhibits good toughness, allowing it to absorb energy during impact or vibration without fracturing, which is important for structures in seismic areas or under dynamic loads.
Excellent Weldability and Machinability:
Can be easily welded using various welding methods to form complex structures.
Also easy to cut, bend, and machine to meet different design and construction requirements.
Dimensions & Tolerance of ASTM A500/A500M tubing

Comparison Table
| Grade | Tensile Strength (minimum) | Yield Strength (minimum) | Elongation (2″) Round | Elongation (2″) Shaped |
| A | 45,000 psi or 310 MPa | 33,000 psi or 228 MPa | 25% | 21% |
| B | 58,000 psi or 400 MPa | 42,000 psi or 290 MPa | 23% | 21% |
| C | 62,000 psi or 427 MPa | 46,000 psi or 317 MPa | 21% | 21% |
| D | 65,000 psi or 448 MPa | 50,000 psi or 345 MPa | 20% | 20% |
Chemical Composition
| Element Name | Grade A (Max %) | Grade B (Max %) | Grade C (Max %) | Grade D (Max %) |
| Manganese | 1.00% | 1.00% | 1.35% | 1.50% |
| Carbon | 0.26% | 0.26% | 0.23% | 0.20% |
| Phosphorus | 0.04% | 0.04% | 0.04% | 0.04% |
| Sulfur | 0.05% | 0.05% | 0.05% | 0.05% |
| Silicon | 0.10% – 0.30% | 0.10% – 0.30% | 0.10% – 0.30% | 0.10% – 0.30% |
Test and inspection

Packaging and shipping