Aug 29, 2025 Leave a message

About S31059 Steel Pipe


1. Material Definition and Composition
S31059 is a high-purity austenitic heat-resistant stainless steel (corresponding to European designation 1.4835). Its core design features include:

High chromium-nickel base (Cr 24.0-26.0%, Ni 19.0-22.0%) provides extreme oxidation resistance;
Ultra-low carbon and high purity (C ≤ 0.025%, P ≤ 0.020%, S ≤ 0.005%) eliminates the risk of sensitization;
Nitrogen fortification (N: 0.15-0.25%) enhances high-temperature strength.
Compliant standards: EN 10216-5 (European standard), ASTM A312 (American standard optional). 2. Performance Advantages and Limit Parameters
Temperature Limit:
Continuous use temperature 1200°C (short-term 1300°C);
Oxidation weight gain at 1150°C <0.5 mg/cm² (100 hours);
Mechanical Properties:
Room temperature tensile strength ≥600 MPa, 800°C strength ≥150 MPa;
-196°C impact energy ≥80 J (potential for low-temperature applications).
3. Typical Industrial Applications
High-temperature industrial furnaces:
Slide rails for billet heating furnaces, heat-resistant components for roller-hearth furnaces;
Glass melting furnace burner sleeves;
Energy:
Molten salt reactor main circuit piping;
Supercritical CO₂ Brayton cycle heat exchange tubes.
4. Comparison with Similar Materials:
vs. S31008 (310S):
Nitrogen addition increases high-temperature strength by 30%;
Ultra-low carbon design improves post-weld corrosion resistance;
vs. RA253MA:
No rare earth addition, 25% cost reduction;
Comparable thermal fatigue resistance. 5. Purchasing and Processing Key Points
Key Tests:
Ferrite content ≤ 0.5% (to prevent sigma phase embrittlement);
1200°C/100-hour oxidation test;
Processing Warnings:
Hot forming requires argon shielding (to prevent surface decarburization);
Welding must use ER310 welding wire with 100% inert gas shielding.