16Mo3 Boiler Steel Pipe: Composition, Properties and Applications

16Mo3 Boiler Steel Pipe: Composition, Properties and Applications

16Mo3 is a low-alloy molybdenum steel for elevated-temperature service, defined in the European standard EN 10216-2 for seamless steel tubes for pressure purposes and in EN 10028-2 for pressure-vessel plates. Its material number is 1.5415. The "16" indicates a nominal carbon content of 0.16%, and the "Mo" signals the deliberate molybdenum addition that gives the steel its creep resistance and high-temperature strength. Although it is sometimes loosely described as a boiler carbon steel, 16Mo3 is a molybdenum-alloy steel, not a plain carbon grade.

Chemical Composition (per EN 10216-2)

Element Content, %
Carbon 0.12 - 0.20
Silicon, max 0.35
Manganese 0.40 - 0.90
Phosphorus, max 0.025
Sulfur, max 0.010
Chromium, max 0.30
Molybdenum 0.25 - 0.35
Nickel, max 0.30
Copper, max 0.30

The controlled carbon window keeps the steel weldable, while molybdenum raises the strength at temperature and improves resistance to creep and to hydrogen attack.

Mechanical Properties (Normalized Condition)

Property Value
Yield Strength Rp0.2, min (t ≤ 16 mm) 270 MPa
Tensile Strength Rm 450 - 600 MPa
Elongation A, min 22%

Yield strength decreases with increasing wall thickness, as defined in the thickness tables of EN 10216-2. Elevated-temperature yield values for design are given in the standard for the design calculation.

Heat Treatment and Processing

The normal delivery condition is normalized, typically around 890-950°C followed by air cooling

Hot forming should finish above the transformation range; after hot forming below about 900°C, re-normalizing is recommended

Cold forming is acceptable within the limits of the standard, followed by the required heat treatment if deformation exceeds the code limit

Welding is performed with low-hydrogen consumables; preheat is generally applied for thicker sections, and post-weld heat treatment around 580-620°C is used when required by the fabrication code

Applications

16Mo3 is specified for boiler and pressure equipment operating at temperatures where plain carbon steel loses strength, typically in the range of 400-500°C. Typical duties include:

Boiler tubes, superheater tubes and steam piping

Boiler headers and collectors

Heat exchangers in refinery and chemical service

Pressure vessels and steam drums built to EN 13445 or the applicable code

Frequently Asked Questions

Q1: What is 16Mo3?
16Mo3 is a molybdenum-alloy steel for elevated-temperature pressure service, defined in EN 10216-2 (tubes) and EN 10028-2 (plates), with material number 1.5415.

Q2: Is 16Mo3 a carbon steel?
It is a low-alloy steel: the molybdenum addition of 0.25-0.35% is what gives it high-temperature strength and creep resistance beyond plain carbon steel.

Q3: What are the mechanical properties of 16Mo3?
In the normalized condition, minimum yield 270 MPa (t ≤ 16 mm), tensile 450-600 MPa and minimum elongation 22%.

Q4: What is the delivery condition of 16Mo3 pipe?
The standard delivery condition is normalized; other conditions can be agreed between buyer and mill.

Q5: Can 16Mo3 be welded?
Yes, with qualified procedures and low-hydrogen consumables. Preheat is applied for thicker sections and PWHT is used where the fabrication code requires it.

Q6: What temperature range is 16Mo3 suitable for?
It is typically used up to about 500°C for pressure parts; the exact design limit comes from the elevated-temperature yield data in EN 10216-2 and the applicable design code.

Send Inquiry