1. Material Definition and Standard Specifications
07Cr17Ni11Ti is a titanium-stabilized austenitic stainless steel (equivalent to US grade 321). Its core properties are:
Composition Design:
The chromium-nickel base (Cr 16.0-18.0%, Ni 10.0-12.0%) provides basic corrosion resistance;
The titanium addition (Ti ≥ 5 × C%, typically 0.30-0.60%) fixes carbon, completely eliminating the risk of intergranular corrosion;
Implementation Standards: GB/T 14976 (National Standard), ASTM A312 (American Standard);
Low Carbon Control: C ≤ 0.08%, P ≤ 0.045%, S ≤ 0.030%
2. Core Performance Advantages
Corrosion Resistance:
Passed the GB/T 4334 E intergranular corrosion test (nitric acid + fluoride environment);
Pitting Resistance Equivalent (PREN) ≥ 18, suitable for weakly acidic media;
High-Temperature Performance:
Continuous operating temperature 800°C (short-term resistance 900°C);
Oxidation resistance superior to 304 stainless steel (oxidation weight gain reduced by 30% at 800°C);
Processing Characteristics:
No preheating required for welding (carbon equivalent CEV < 0.35%);
Annealing required after cold forming (rapid cooling at 1010-1120°C).
3. Typical Applications
Petrochemical Equipment:
Catalytic Cracking Unit Reactor Piping;
Sour Oil and Gas Pipelines;
Energy:
Nuclear Power Plant Secondary Circuit Heat Exchanger Tubing;
Boiler Flue Gas Waste Heat Recovery Systems;
Special Requirements:
Thin-walled pressure vessels requiring no post-weld heat treatment;
Acidic media containers in food processing equipment. 4. Comparison with Similar Materials
vs 06Cr18Ni11Ti (321H):
Lower carbon content, lower risk of sensitization in the heat-affected zone of welding;
Similar cost, but slightly inferior high-temperature stability;
vs 07Cr17Ni12Mo2 (316):
No molybdenum added, weaker resistance to chloride corrosion;
15-20% lower price, better cost-performance.
5. Procurement and Processing Key Points
Key Certificates: Titanium content test report (Ti/C ≥ 5) is required;
Processing Notes:
Carbon steel tools are prohibited for cutting (to avoid iron ion contamination);
Solution treatment is required after hot forming;